PLA-Guard is designed specifically for antibacterial needs

Antibacterial material

Contains special glass powder that can slowly release zinc ions, which can effectively inhibit the growth of bacteria such as Staphylococcus aureus and Escherichia coli.

High printing speed

Printing speeds up to 600 mm/s, good adhesion between layers, fast heating flow, fast cool-forming rate without printheads nozzle clogging.The mechanical properties of the filament and fast printing performance is well-balanced.

Quality control

Trouble-free printing can be achieved by the filament with a smooth and even surface, uniform diameter, good winding arrangemet.

Product Safety

Comply with RoHS and REACH regulations

PLA-Guard is designed specifically for antibacterial needs

Antibacterial material

Contains special glass powder that can slowly release zinc ions, which can effectively inhibit the growth of bacteria such as Staphylococcus aureus and Escherichia coli.

High printing speed

Printing speeds up to 600 mm/s, good adhesion between layers, fast heating flow, fast cool-forming rate without printheads nozzle clogging.The mechanical properties of the filament and fast printing performance is well-balanced.

Quality control

Trouble-free printing can be achieved by the filament with a smooth and even surface, uniform diameter, good winding arrangemet.

Product Safety

Comply with RoHS and REACH regulations

Pruduct_BannerPruduct_BannerPruduct_BannerPruduct_BannerPruduct_Banner

Net Weight

1 kg

Wire Diameter

1.75 ± 0.03 mm

Printing Speed

150 ~ 600 mm/s

Bending Strength (X-Y)

72 Mpa

Tensile Strength (X-Y)

41 Mpa

Printing Temperature

190 ℃ ~ 230 ℃

Storage condition

Please store the material in a cool, dry place, prolonged exposure to moisture will damage the performance of the material.